SEM x1000

Figure 3. At 1000X we can begin to see the boundaries between the pockets of liquid phase sintering additive and the zirconia matrix. The small, light particles are zirconia particles exposed by the polishing process.

SPECIMEN PREPARATION

ETCHING PROCEDURE

ZRO2_HOME