SEM x5000

Figure 4. At 5000X a pocket of sintering additive in the zirconia matrix is clearly visible. This additive is a liquid at the sintering temperature. Upon cooling it shrinks more than the surrounding matrix. This leads to the cracking observed at the boundary as the shrinking additive phase tries to pull away from the matrix.

SPECIMEN PREPARATION

ETCHING PROCEDURE