SEM x200

Figure 2. After firing at 1000C for four hours this SEM micrograph shows the distribution of zirconia ( light gray phase) and sintering additives ( darker phase). The additives are uniformly dispersed in the zirconia matrix.

SPECIMEN PREPARATION

ETCHING PROCEDURE