Optical x100

Figure 1. This low magnification micrograph shows the structure that results from firing the green ceramic at 1000C for two hours. The white phase is zirconia. The dark phase is small pockets of sintering additives plus porosity.

SPECIMEN PREPARATION

ETCHING PROCEDURE

ZRO2_HOME